Material Characteristics


Material Characteristics
Material Properties Symbol Unit Measuring Conditions SFP3 SFP4 SFP41 SFP42 SFP5 SFA43 SFA05 SFA07 SFA10 SFA121 SFA151 SFN4 SFN41
Freq. Flux den. Temp.
Initial Permeability μi   10kHz 0.25mT 25°C 2000±25% 2300±25% 2400±25% 1800±25% 2000±25% 4500±25% 5000±25% 7000±25% 10000±30 12000±30% 15000±30% 2500±25% 2500±25%
Power Loss Pv kW/m3 25kHz 200mT 25 °C     125 125                  
100°C 155   50 50                  
100kHz 200mT 25 °C   650 650 750                  
100°C 920 410 350 350                  
300kHz 100mT 25 °C     820 900 600                
100°C     500 500 450                
500kHz 50mT 25 °C     400 450 220                
100°C     300 300 250                
Saturation Flux Density Bms mT 10KHz H=1200A/m 25°C 500 510 495 520 470 460 440 400 410 380 400 450 450
100°C 410 390 395 420 350 300 300 200 210 180 170 320 320
Remanence Brms mT 10KHz H=1200A/m 25°C   100 170 200 100 65 80 150 140 130 220 90 90
100°C   55 70 70 60 60 90 110 110 110 100 100 100
Coercivity Hc A/m 10kHz H=1200A/m 25°C 23 14 11 12 12                
100°C 19   6 6 8                
Relative Loss Factor tanδ /µi 10-6 10KHz <0.25mT 25°C           <10 <4 <8 <10 <10 <10 <7 <7
100kHz 25°C           <10 <15 <30 <60 <60 <110 <3 <3
Hysteresis Material Constant ηB 10-6/mT 10KHz 1.5-3.0mT 25°C <1.5 <1.2 <1.0 <1 <1 <0.5 <0.8 <1.2 <0.5 <0.5 <0.5 <0.6 <0.6
Disaccommodation Factor DF 10-6 10KHz < 0.25mT 25°C   <2 <2.0 <2 <2 <2 <3 <2 <2 <2 <2    
Curie Temperature Tc °C       >220 220 230 240 220 160 140 130 130 110 110 170 170
Resistivity ρ Ωm       3 6.5 4 8 6.4 0.2 0.2 0.35 0.15 0.12 0.1 7.5 7.5
Density d g/cm3       4.8 4.8 4.85 4.9 4.7 4.85 4.85 4.9 4.9 4.9 5.0 4.7 4.7